1. Product Introduction:
D001 FG It is a macroporous strong acid cation exchange resin with a polystyrene skeleton, containing sulfonic acid groups, equivalent to solid sulfuric acid. It has uniform pore size, high mechanical strength, and high hydrogen form rate, mainly used for high-speed mixed bed water treatment.
Corresponding foreign brands: Amberlite 200, Lewatit Sp-210
2. Performance Indicators:
Appearance
Light brown opaque spherical particles
Functional Group
-SO3H
Delivery Form
Na+
Total Exchange Capacity
≥4.35 mmol/g
Volume Exchange Capacity
≥1.8 mmol/ml
Moisture Content
45%~55%
Wet True Density
1.25~1.28 g/ml
Wet Apparent Density
0.77~0.85 g/ml
Particle Size Range
0.315~1.25 mm
Effective Particle Size
0.40-0.70mm
Uniformity Coefficient
≤1.6
Abrasion and Roundness Rate
≥90%
Color
≤25APHA
3. Reference Operating Conditions:
Maximum Operating Temperature
120℃
Resin Bed Height
1~3 m
Operating Flow Rate
2~10 BV/h
Backwash Flow Rate
4~10 BV/h
Regeneration (Desorption) Flow Rate
1~2 BV/h
Regenerant Dosage
2 BV 3~5% HCl, 2 BV 2~4% NaOH
4. Product Applications:
Mainly used for high-speed mixed bed water treatment, precious metal recovery, and organic catalytic reactions.
5. Precautions:
1. Transportation and Storage of the Product:
The product should be stored wet, preferably at temperatures above 0°C; if unused for a long time, it can be sealed or immersed in 5% the above brine; during transportation, anti-freezing is the main concern, and heavy objects should not be placed on the resin to prevent crushing.
2. Resin Pretreatment:
Generally, alkaline -water - acid - water treatment in one process is acceptable; for strict requirements, three cycles should be performed, finally treating to the required ion form.
3. Resin Loading:
Consider the resin's swelling rate during ion exchange, reserve enough space to prevent overflow and ensure appropriate liquid level; the column diameter ratio should be reasonable to avoid channeling; use wet loading or backwash to remove air bubbles inside the resin bed.
4. Before liquid enters the resin column, it should undergo flocculation, filtration, or sand filtration to ensure no suspended solids, preventing blockage of resin pores.
5. Resin unused in the column for a long time should be cleaned and removed for storage, or immersed in saltwater in a salt-resistant medium, keeping the surface from dehydration; periodic backwashing is also needed to loosen the resin and prevent caking and spoilage.
D001FG
You can also leave us a message to get the latest product information!
Similar Products:
Product Keywords:
Consult Now
If you are interested in our products, please leave your email, and we will contact you as soon as possible, thank you!